Annealing 96COE
What is the schedule to anneal beads made from 96 COE rods? I'm starting to experiment with this glass and can't find any information on annealing schedules.
|
Same as 104
|
Great. Thank you.
|
Spectrum recommends 510˚C for it's 96 glass
Bullseye recommends 482˚C for it's 90 glass Effetre recommends 470˚C for it's 104 glass I hope this is of some use to you, cheers, B |