My kiln is brick and I never put kiln wash on my kiln, its just more dirty dusty stuff in the kiln.

For soft glass fussing and slumping and boro slumping I use a kiln shelf and use kiln wash only on the top of the shelf.

I slump boro for fun sometimes 30 minutes at 1,600f and things flatten out nice.