Quote:
Originally Posted by Moth
I use non-sudsing ammonia in my ultrasonic and I've never had trouble with dull reduction glass. I cut it with water about 2:1...maybe that helps?
Great idea, Mark. You are pretty sharp.
~~Mary
|
Cool, good to know Mary.
Maybe ammonia doesn't have the same problem that I've seen with vinegar? I just figured that it was an acid so it would have the same effect. Could just be a matter of how long it stays in there.. We can always experiment with some reject beads or just a reduced piece of stringer.
__________________
To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts. (Beau & Shani)
To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.
To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.
To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.
To view links or images in signatures your post count must be 5 or greater. You currently have 0 posts.
|