This is my second post so I am not sure if I am doing this correct. I LOVE all of the tips, thank you. I have more confidence now knowing I can get excited if I only have 3 beads that look good out of the many I made. I am really confused about annealing times. I use a King Pin digital controlled kiln. The supplier told me 940 degrees was sufficient. However, when I bought my first supply of Lausha from flamedame.com there was a different annealing schedule that goes to 980 and a longer annealing time than I was doing. It also had a slower ramp down. Well, when I combine colors, especially silver glass, I mess the color up. My silver pink turned purple. So can someone please advice me on Proper Annealing and should I be mixing Lausha with other glass like Effetre?